Customization: | Available |
---|---|
Usage: | Packaging Film |
Type: | Metallized Film |
Still deciding? Get samples of $ !
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Item | Standard | Measurement | |
Net weight | Net weight±0.2kg( not including roll core) | Platform scales | |
Apparent Mass | The surface of products must be clean, aluminized coating uniform, no pollution,smell and damage. | Ruler and eyes | |
Width | Conform to the Order Diagonal tolerance≤2mm | Ruler,film size | |
Thickness | (base film thickness 15μm±1μm) | Thickness tester | |
Shimline | shimless | By eyes | |
Surface Tension | ≥38 Dnye | Dnye tester | |
Compound fastness | Use tape to pull the aluminum layer, no aluminum off by 180 Degree pulling | Tape | |
Film length &joint | 6000+50m/per roll,joint≤2 /roll( Or 12000+100m,Joint≤4/per roll),joint interval≥500m.Use yellow tape to mark on joint place. | By eyes |
|
Strap | Obvious strap is less no 1/per circle,strap width<0.1mm,acceptable after printing. |
|
|
Brightspot/ Dark spot |
Bright spot or dark spot (φ≤0.2mm) cannot be dense; Bright spot or dark spot (0.2<φ≤0.3mm) acceptable qty is 5 pics in one plate circle Bright spot or dark spot (0.3<φ≤0.5mm) acceptable qty is 3 pics in one plate circle Bright spot or dark spot(φ>0.5mm) is not acceptable |
||
brightness/ aberration | 1. film surface hue is according to samples, △L*≤±2.0. 2. brightness and hue on joint are relatively similar. |
||
interference fringe | No obvious shimless rainbow film, no obvious interference fringe and shim line mark | ||
Bright line/ scratch | Light line is acceptable if it cannot be easy found after printing: Light line and invisible scratch is acceptable |
||
Dark line/dark spot | Tiny dark line/light spot is acceptable if they are not easy found after printing | ||
Crack coating | Light crack coating on partial film is acceptable, but serious crack coating is not acceptable | ||
Others | Core Dia:3 " |